Abstract
To enhance Li storage properties, nitrogenation methods are developed for Si anodes. First, melamine, urea, and nitric oxide (NO) precursors are used to nitrogenize carbon-coated Si particles. The properties of the obtained particles are compared. It is found that the NO process can maximize the graphitic nitrogen (N) content and electronic conductivity of a sample. In addition, optimized N functional groups and O─C species on the electrode surface increase electrolyte wettability. However, with a carbon barrier layer, NO hardly nitrogenizes the Si cores. Therefore, bare Si particles are reacted with NO. Core-shell Si@amorphous SiNx particles are produced using a facile and scalable NO treatment route. The effects of the NO reaction time on the physicochemical properties and charge–discharge performance of the obtained materials are systematically examined. Finally, the Si@SiNx particles are coated with N-doped carbon. Superior capacities of 2435 and 1280 mAh g−1 are achieved at 0.2 and 5 A g−1, respectively. After 300 cycles, 90% of the initial capacity is retained. In addition, differential scanning calorimetry data indicate that the multiple nitrogenation layers formed by NO significantly suppress electrode exothermic reactions during thermal runaway.
Original language | English |
---|---|
Article number | 2310062 |
Journal | Advanced Science |
Volume | 11 |
Issue number | 25 |
DOIs | |
Publication status | Published - 2024 Jul 3 |
All Science Journal Classification (ASJC) codes
- Medicine (miscellaneous)
- General Chemical Engineering
- General Materials Science
- Biochemistry, Genetics and Molecular Biology (miscellaneous)
- General Engineering
- General Physics and Astronomy