HYDROTHERMAL CRYSTALLIZATION AND CRYSTAL GROWTH OF UN-DOPED AND ZrO2-DOPED CeO2.

Eiji Tani, Masahiro Yoshimura, Shigeyuki Somiya

Research output: Contribution to journalArticlepeer-review

Abstract

Crystallization was studied on precipitated hydrous ceria with KF, LiCl, LiBr, K//2CO//3, LiNO//3, Li//2SO//4 and NaOH solutions under 100 MPa at 500 to 600 degree C for 24h. The KF and Li//2SO//4 solutions enhanced growth of un-doped CeO//2. The LiCl, LiBr and Li//2SO//4 solutions enhanced growth of ZrO//2-doped CeO//2. Calcination contributed to the hydrothermal growth of ZrO//2-doped CeO//2 with LiCl solution. Single crystals of un-doped CeO//2 and ZrO//2-doped CeO//2 were obtained by hydrothermal treatments with KF and LiCl solutions, respectively.

Original languageEnglish
Pages (from-to)47-53
Number of pages7
JournalReport of the Research Laboratory of Engineering Materials Tokyo
Issue number8
Publication statusPublished - 1983 Jan 1

All Science Journal Classification (ASJC) codes

  • Engineering(all)

Fingerprint Dive into the research topics of 'HYDROTHERMAL CRYSTALLIZATION AND CRYSTAL GROWTH OF UN-DOPED AND ZrO<sub>2</sub>-DOPED CeO<sub>2</sub>.'. Together they form a unique fingerprint.

Cite this