Abstract
Hydroxyapatite ceramics with zirconia dispersion from fine powders synthesized hydrothermally were post-sintered at 1000-1300°C under 200 M Pa of argon for 1 h without capsules, after normal sintering in air at 1200°C for 3 h. Densification was most significant with post-sintering at 1200°C. Fracture toughness, Vickers hardness and elastic properties of these materials were investigated. Post-sintering gave twice the K1c value of transparent pure hydroxyapatite ceramics. Vickers hardness and Young's modulus of the ceramics were increased by post-sintering.
| Original language | English |
|---|---|
| Pages (from-to) | 57-61 |
| Number of pages | 5 |
| Journal | Biomaterials |
| Volume | 11 |
| Issue number | 1 |
| DOIs | |