Abstract
The mesoporous silica submicron-spheres (80-200 nm) with a small dispersion in diameter (<10%) as the building blocks of the artificial mesoporous silica opals have been synthesized using quaternary ammonium surfactant as template in an aqueous solution of suitable polarity at near neutral condition of pH = 7.0-9.0.
Original language | English |
---|---|
Pages (from-to) | 838-839 |
Number of pages | 2 |
Journal | Chemistry Letters |
Volume | 33 |
Issue number | 7 |
DOIs | |
Publication status | Published - 2004 Jul 5 |