AZO electrodes deposited by atomic layer deposition for OLED fabrication

B. Dugrenil, I. Séguy, Hsin Ying Lee, T. Camps, Y. C. Lin, J. B. Doucet, Y. S. Chiu, L. Salvagnac, E. Bedel-Pereira, M. Ternisien, C. T. Lee, V. Bardinal

研究成果: Conference contribution

1 引文 斯高帕斯(Scopus)

摘要

In this work, we present a comparative study of optimized AZO electrodes deposited by Atomic Layer Deposition (ALD) with commercial ITO in terms of electrical, optical and structural properties. Despite a lower figure of merit mainly due to a higher sheet resistance, AZO-based OLEDs are shown to present a current density five times higher than ITO-based ones for the same applied voltage. These AZO electrodes fabricated by ALD could thus be promising substitutes for conventional ITO anodes in organic electronic devices.

原文English
主出版物標題Organic Photonics VI
發行者SPIE
ISBN(列印)9781628410853
DOIs
出版狀態Published - 2014
事件Organic Photonics VI - Brussels, Belgium
持續時間: 2014 四月 152014 四月 16

出版系列

名字Proceedings of SPIE - The International Society for Optical Engineering
9137
ISSN(列印)0277-786X
ISSN(電子)1996-756X

Other

OtherOrganic Photonics VI
國家/地區Belgium
城市Brussels
期間14-04-1514-04-16

All Science Journal Classification (ASJC) codes

  • 電子、光磁材料
  • 凝聚態物理學
  • 電腦科學應用
  • 應用數學
  • 電氣與電子工程

指紋

深入研究「AZO electrodes deposited by atomic layer deposition for OLED fabrication」主題。共同形成了獨特的指紋。

引用此