Effect of CuO additives on sintering and dielectric behaviors of CeO2 ceramics

  • Wen Shiush Chen
  • , Ching Fang Tseng
  • , Yi Mu Lee
  • , Hsin Han Tung
  • , Hong Tzer Yang
  • , Cheng Hsing Hsu

研究成果: Article同行評審

7   !!Link opens in a new tab 引文 斯高帕斯(Scopus)

摘要

The effects of CuO addition (1 and 2 wt%) on microstructures and microwave dielectric properties of CeO2 ceramics with CuO additions have been investigated. It is found that CeO2 ceramics can be sintered at 1490 °C due to the liquid phase effect of CuO addition. At 1580 °C, CeO2 ceramics with 1 wt% CuO addition possesses a dielectric constant (εr) of 21.7, a Q × f value of 50,000 (at 9GHz) and a temperature coefficient of resonant frequency (τf) of -59 ppm/°C. A large sintering temperature reduction (about 200 °C) can be achieved by adding CuO to the CeO2 ceramics. The CuO-added CeO2 ceramics can find applications in microwave devices.

原文English
頁(從 - 到)2277-2281
頁數5
期刊Journal of Materials Processing Technology
209
發行號5
DOIs
出版狀態Published - 2009 3月 1

All Science Journal Classification (ASJC) codes

  • 陶瓷和複合材料
  • 電腦科學應用
  • 金屬和合金
  • 工業與製造工程

指紋

深入研究「Effect of CuO additives on sintering and dielectric behaviors of CeO2 ceramics」主題。共同形成了獨特的指紋。

引用此