HYDRATION OF CALCIUM ALUMINATES (3:1, 12:7, 1:1, 1:2 AND 1:6) IN PHOSPHORIC ACID SOLUTIONS AT VARIOUS TEMPERATURES.

Kengo Yamazaki, Toshihiko Nakazawa, Masahiro Yoshimura, Shigeyuki Somiya

研究成果: Article同行評審

1 引文 斯高帕斯(Scopus)

摘要

The purpose of the work is to obtain information on products in the system CA//n-H//3PO//4(H//2O) and study the influence of phosphoric acid on the hydration of CA//n at various temperatures. A curing temperature of 35 degree C and hydrothermal conditions of 100 degree C and 200 degree C under 10 MPa was used.

原文English
頁(從 - 到)43-53
頁數11
期刊Report of the Research Laboratory of Engineering Materials Tokyo
發行號7
出版狀態Published - 1982 一月 1