Reduction of Micro-Crack in Ni-Based Superalloy IN-713LC Produced by Laser Powder Bed Fusion
- M. Mohsin Raza
- , Hung Yu Wang
- , Yu Lung Lo
- , Hong Chuong Tran
研究成果: Conference contribution